Soda Ash goes sigma mixer through starting of vibroseive or ceiving.Add Common Salt goes directly passing in sigma mixer it means both two soda and common salts goes in sigma mixer through RAW MARERIAL charging tube.Then after start the sigma mixer,spray Sulphonic Acid with colour solution in Acid Tank approximately five minutes with the help of starting of agitator. Later on,Add Catalytic water and Lemon Perfume.
Again take Dolomite and Forca-U in RAW MATERIAL charging chute through directly which is discharged or mixing to each other under 30-45 seconds in mixer.Lastly Filling,Sealing and Stiching.
Again take Dolomite and Forca-U in RAW MATERIAL charging chute through directly which is discharged or mixing to each other under 30-45 seconds in mixer.Lastly Filling,Sealing and Stiching.